Critical Pitting Corrosion Temperature And Critical Crevice Corrosion Temperature Setting | Duplex Steel, Stainless Steel Pipe and Fittings | KAYSUNS
Critical pitting temperature (CPT) refers to the lowest temperature enthalpy at the initiation and development of steady-state pitting on the surface of a sample under specific test conditions.